Teknofay Ceramic Tile Adhesive

Teknofay Ceramic Tile Adhesive
Ceramic Tile Adhesive
  TDS Technical Document Sheet   

  TSE Document   

Product Description
Cement based, ceramic and tile adhesive with high bonding strength and ability to work far a long time.

Areas of Usage 
• It is used in vertical and horizontal applications,
• In houses, shopping malls, hospitals,
• Far adhering materials such as small and medium sized tiles, ceramics with a water absorption rate of over 3%

Features and Benefits
• Easy to prepare and apply.
• It has high adhesion properties.
• It does not slip in vertical applications.
• It saves time and labor.

Application Notes / Restrictions
• lf there is a dusty surface (engop) behind the ceramic, it should be cleaned with a hard brush.
• Prepared mortar is spread to the surface with a notched trowel with a suitable tooth size. On combed mortar. lf the coating materials (ceramic, tiles, ete.) are glued within 15 min. lf this time has passed, the mortar should be scraped off from the surface and from the coatings. it should be applied with ready-made mortar.
• The product may irritate the skin contact. Work clothes, protective gloves, masks and glasses must be used. Protective cream can also be applied before starting work.
• in case of grout contact with eyes, eyes should be washed immediately with warm water and consult a doctor.
• it must be taken under protection of the environment to be below (+) 5 °C, covered with nylon or heat insulation plates should be prevented to expose the product to freezing.
• (+) At temperatures above 35°C, cover with nylon or heat insulation plates to prevent the product from being exposed to sudden water loss.
• At least 24 hours afterthe application ofthe Teknofay, the joint must be filled.
• Do not add foreign matter.
• it must be protected after application against adverse weather conditions such as direct sunlight, high air temperature (above +35 °C), rain and frost. The product should be cleaned thoroughly with water and detergent before it is fully cured and hardened.
• lmmediately after application, before hardened, the equipment should be cleaned with water. After the product is hardened, it should be cleaned by mechanical methods.

Storage Conditions / Shelf Life
it should be stored in original unopened package, in cool and dry environment, protected from freezing.