TDS Technical Document Sheet
|
Product DescriptionAcrylic dispersion polymer based plaster primer for sub-plaster and gypsum surfaces,
horizontal and overhead applications.
Areas of Usage• lt's used indoor, in verticals and ceilings,
• To increase the adherence of gypsum, lime and cement based plaster mortars to the exposed
concrete surface ,
• As primer in ceiling plasters.
Features and Benefits• Creates a strong and permanent bond.
• Easy to be applied.
• Prevents rapid water loss in cement and gypsum based plaster
• High water impermeability.
Application lnstructionsSurface should be solid, free of loose and weak parts, free from freezing, foreign materials and other
pollutants such as cement grout, accumulated water, oil, grease, paraffin, coatings ete. must be
removed and cleaned. The surface should be prepared by suitable mechanical preparation
techniques such as high pressure water or abrasive equipment. AII dust, loose and easily crumbly
materials should be removed completely by brush and / or vacuum before application.
it should be mixed in a clean container, which is free of any kind of antiadhesive substance, in a clean
container or in its own packaging, in a way that it will be homogeneous by using a mixer of low speed
(400-600 rpm) by putting a maximum of 6 liters of water in a 12 kg bucket of TEKNOLATEX 200
Pro. TEKNOLATEX 200 Pro should be mixed at regular intervals while working. Apply to the surface
by brush, roller and spray.
Application Notes / Restrictions• The product may be irritating to the skin. Work clothes, protective gloves, masks and glasses
must be used. Protective cream can also be applied before starting work. in case of mortar
contact with eyes, eyes should be washed immediately with warm water and consult a doctor.
• Do not add foreign substances.
• Pretesting is recommended for different applications.
• it must be protected after application against adverse weather conditions such as direct
sunlight, high air temperature (above +35° C), rain and frost. The product should be cleaned
thoroughly with water and detergent before it is fully cured and hardened.
• lmmediately after application, before hardened, the equipment should be cleaned with water.
After the product is hardened, it should be cleaned by mechanical methods.